Resin-dentin bond stability and physical characterization of a two-step self-etching adhesive system associated with TiF4

Texto completo
Autor(es):
Torres, Gabriele Barbosa [1] ; da Silva, Tania Mara [2] ; Basting, Rosanna Tarkany [3] ; Bridi, Enrico Coser [1] ; Gomes Franca, Fabiana Mantovani [1] ; Turssi, Cecilia Pedroso [1] ; Botelho do Amaral, Flavia Lucisano [1] ; de Paiva Goncalves, Sergio Eduardo [2] ; Basting, Roberta Tarkany [1]
Número total de Autores: 9
Afiliação do(s) autor(es):
[1] Sao Leopoldo Mand Dent Sch & Res Ctr, Rua Jose Rocha Jungueira 13, BR-13045755 Campinas, SP - Brazil
[2] UNESP Univ Estadual Paulista, Inst Sci & Technol Sao Jose dos Campos, Ave Engenheiro Francisco Jose Longo 777, BR-12245000 Sao Jose Dos Campos, SP - Brazil
[3] Univ Campinas UNICAMP, Fac Med Sci FCM, Rua Tessalia Vieira Camargo, BR-13083887 Campinas, SP - Brazil
Número total de Afiliações: 3
Tipo de documento: Artigo Científico
Fonte: Dental Materials; v. 33, n. 10, p. 1157-1170, OCT 2017.
Citações Web of Science: 5
Resumo

Objectives. To evaluate the bond strength to superficial (SD) and deep (DD) dentin after the use of 2.5% (T2.5%) or 4% (T4%) titanium tetrafluoride (TiF4) in aqueous solution as a dentin pretreatment, or when incorporated into the primer (T2.5%P and T4%P) of an adhesive system (Clearfil SE Bond/CL). Degree of conversion (DC), particle size (PS), polydispersity index (PI) and zeta potential (ZP) of the solutions were evaluated. Methods. Fifty molars were sectioned longitudinally to obtain two slices of each tooth, which were demarcated into SD and DD. Treatments were applied (n = 10): CL; T2.5%; T4%; T2.5%P; T4%P. After 24 h or 180 days storage, microshear bond strength tests were performed. The DC values of T2.5%P and T4%P were evaluated by FTIR. PS, PI and ZP were measured using dynamic light scattering. Results. Analysis of mixed models showed significant effect of concentration of TiF4 {*} solution {*} storage time (p = 0.0075). There were higher bond strength values in SD than in DD (p = 0.0105) for all treatments in both times. The failure mode showed adhesive failures in the majority of groups, irrespective of depth and time (p = 0.3746). The bond strength values were not affected by treatments. Lower average particle size was observed for T2.5%P and T4%P at baseline. T2.5% and T4% showed a trend towards agglomeration. Signcance. Higher bond strength values were achieved at SD for all treatments and times. The failure modes observed were adhesive. TiF4 incorporation did not affect DC. T2.5%P and T4%P presented excellent stability over time. (C) 2017 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved. (AU)