Abstract
The aim of this study is to investigate the corrosive behavior of commercially-pure titanium (cpTi) discs as a function of different surface modifications: machined (surface I - control), modified by chloride acid and hydrogen peroxide (surface II), modified by sulfuric acid and hydrogen peroxide (surface III), modified by aluminum oxide sandblasting (surface IV) followed by chloride acid…